- Anion-exchange membrane
- Thickness: 80 µm
- Basis weight: ∼90 g/m²
- Ultimate Tensile Strenght: >80 MPa
- Elongation at Break: >40%
- IEC (OH– , meq/g): >2.0
- Conductivity (mS/cm, OH– , RT): >50
- H2 Permeance (mA/cm²bar, HCO3-, 60 °C): <0.30
- High performance, low crossover, high pressure operation, high mechanical strength
- Swelling Ratio (X,Y%, 80 °C, 1 M KOH): ∼10
- Swelling Ratio (Z%, 80 °C, 1 M KOH): ∼30
- Water Uptake (%, 80 °C, 1 M KOH): ∼60
- AEM Electrolyzer